Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 5.16 J/cm | 9.67 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP RX85514 PA 66 LNP LUBRICOMP* RX85514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 5.16 J/cm | 9.67 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP RX88514 PA 66 LNP LUBRICOMP* RX85514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). AddedLNP LUBRICOMP* RX85514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). A.. |
|||
Izod Impact, Unnotched | 5.16 J/cm | 9.67 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP ZFL34 PPE+PS LNP* LUBRICOMP* ZFL34 is a compound based on PPE+PS resin containing 20% Glass Fiber, 15% PTFE. Added feature of this gradae is: Wear Resistant. |
|||
Izod Impact, Unnotched | 5.16 J/cm @Temperature 23.0 °C |
9.67 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Lubricomp ZFL34 PPO LNP* Lubricomp* ZFL34 is a compound based on Modified PPO containing glass fiber and PTFE.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 5.16 J/cm @Temperature 23.0 °C |
9.67 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp RF004S PA 66 LNP* Thermocomp* RF004S is a Nylon 6/6 containing Glass Fiber. Characteristics are Heat Stabilized.This data was supplied by SABIC-IP for the Americas region. |