Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 4.33 J/cm | 8.11 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON DEL139P PC LNP* STAT-KON* DEL139P is a compound based on Polycarbonate containing 15% Carbon Fiber, 5% PTFE. Added features of this grade include: Electrically Conductive, Exceptional Processing, Flame Retar.. |