Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 4.11 J/cm | 7.70 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON DEP23FXC PC LNP STAT-KON* DEP23FXC is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 10% PTFE/Silicone. Added features include: Electrically Conductive. Wear Resistant, Superior Molding. |
|||
Izod Impact, Unnotched | 4.11 J/cm @Temperature 23.0 °C |
7.70 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp EB004 PEI LNP* Thermocomp* EB004 is a compound based on Polyetherimide resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 4.11 J/cm @Temperature 23.0 °C |
7.70 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp EB004 PEI (Asia Pacific) LNP* Thermocomp* EB004 is a compound based on Polyetherimide resin containing Glass Bead.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Unnotched | 4.11 J/cm | 7.70 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP UF006AS PPA LNP THERMOCOMP* UF006AS is a compound based on Polyphthalamide resin containing 30% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Unnotched | 4.11 J/cm | 7.70 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON DEP23FXC PC (Asia Pacific) LNP STAT-KON* DEP23FXC is a compound based on Polycarbonate resin containing Silicone, Carbon Fiber, PTFE. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched | 4.11 J/cm | 7.70 ft-lb/in | ASTM D4812 |
A. Schulman SCHULAMID® 66 GF13 13% Glass Fiber Reinforced Nylon 66 Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 4.11 J/cm | 7.70 ft-lb/in | ASTM D4812 |
A. Schulman SCHULAMID® 66 GF13 13% Glass Fiber Reinforced Nylon 66 Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 4.11 J/cm | 7.70 ft-lb/in | ASTM D4812 |
A. Schulman SCHULAMID® 66 GF13 13% Glass Fiber Reinforced Nylon 66 Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 4.11 J/cm | 7.70 ft-lb/in | ASTM D4812 |
A. Schulman SCHULAMID® 66 GF13 13% Glass Fiber Reinforced Nylon 66 Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 4.11 J/cm | 7.70 ft-lb/in | ASTM D4812 |
A. Schulman SCHULAMID® 66 GF13 13% Glass Fiber Reinforced Nylon 66 Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 4.11 J/cm | 7.70 ft-lb/in | ASTM D4812 |
A. Schulman SCHULAMID® 66 GF13 13% Glass Fiber Reinforced Nylon 66 Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 4.11 J/cm @Thickness 3.18 mm |
7.70 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Thermocomp® UF-1006 A HS Polyphthalamide, Glass Fiber Reinforcement
(discontinued **) Features: Heat StabilizedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are sti.. |