Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 3.82 J/cm @Temperature 23.0 °C |
7.16 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp RFZ71S PA 66 LNP* Thermocomp* RFZ71S is a compound based on Nylon 66 resin containing Glass Fiber, Milled Glass. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for t.. |
|||
Izod Impact, Unnotched | 3.82 J/cm @Temperature 23.0 °C |
7.16 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp RFZ71S PA 66 (Asia Pacific) LNP* Thermocomp* RFZ71S is a compound based on Nylon 66 resin containing Glass Fiber, Milled Glass. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for t.. |