Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 3.47 - 8.01 J/cm | 6.50 - 15.0 ft-lb/in | Average value: 5.06 J/cm Grade Count:16 |
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar.. |
|||
Izod Impact, Unnotched | 3.47 J/cm @Temperature 23.0 °C |
6.50 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Lubricomp KZL34 POM LNP* Lubricomp* KZL34 is a compound based on Acetal resin containing Milled Glass and PTFE. Characteristic of this grade is Internally Lubricated.This data was supplied by SABIC-IP for the Americas.. |
|||
Izod Impact, Unnotched | 3.47 J/cm | 6.50 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP RP004 PA 66 (Asia Pacific) LNP* Lubricomp* RP004 is a compound based on Nylon 66 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 3.47 J/cm | 6.50 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON Cycoloy_JK800 PC+ABS LNP* Stat-kon* Cycoloy_JK800 compound is an 8% carbon fiber reinforcedPC+ABS, electrostatic dissipative ECO conforming FR. Good hydrolytic stability. |
|||
Izod Impact, Unnotched | 3.47 J/cm @Thickness 3.17 mm |
6.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Electrablend® PC NCF15 FR 15% Nickel-Coated Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Nickel-Coated Carbon Fiber Reinforcement, 20% Filler by WeightFeatures: Electromagnetic Shielding (EMI) and Flame RetardantInformation .. |
|||
Izod Impact, Unnotched | 3.47 J/cm @Thickness 3.17 mm |
6.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® ABS E GM15 LE 15% Glass Filled Availability: North AmericaFeatures: Low ExtractablesForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 3.47 J/cm @Thickness 3.17 mm |
6.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® ABS GF15 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightFeatures: Good FlowInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 3.47 J/cm | 6.50 ft-lb/in | ASTM D256 |
Spartech SP-9080 High Heat ABS Sheet Description: ABS SheetInformation provided by Spartech. |
|||
Izod Impact, Unnotched | 3.47 J/cm @Temperature 23.0 °C |
6.50 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Stat-kon NX03602 PC+ABS LNP STAT-KON* NX03602 is a compound based on PC+ABS Blend resin containing Carbon Fiber, Flame Retardant. Added features of this material include: Electrically Conductive.This data was supplied by .. |
|||
Izod Impact, Unnotched | 3.47 J/cm @Thickness 3.17 mm |
6.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PP GF10 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 3.47 J/cm @Thickness 3.17 mm |
6.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Statiblend® ABS GF15 AS 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 15% Filler by WeightAdditive: AntistaticFeatures: AntistaticInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 3.47 J/cm @Temperature 23.0 °C |
6.50 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp PH0600B PA 6 (Asia Pacific) LNP* Thermocomp* PH0600B is a compound based on Nylon 6 resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by SABIC.. |
|||
Izod Impact, Unnotched | 3.47 J/cm @Thickness 3.17 mm |
6.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® ABS GF20 BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAppearance: BlackTPCI# 9822121Information provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 3.47 J/cm @Thickness 3.17 mm |
6.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® ABS GF20 LE 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightFeatures: Low ExtractablesInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 3.47 - 5340 J/cm | 6.50 - 10000 ft-lb/in | Average value: 6.69 J/cm Grade Count:47 |
Overview of materials for Acetal Copolymer, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Izod Impact, Unnotched | 3.47 - 8.54 J/cm | 6.50 - 16.0 ft-lb/in | Average value: 5.84 J/cm Grade Count:14 |
Overview of materials for Polybutylene Terephthalate (PBT), PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), PTFE Filled". Each property range of values reported is minimum and ma.. |