Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 3.46 J/cm | 6.48 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON EX11402 PEI LNP* STAT-KON* EX11402 is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |