Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 3.37 J/cm | 6.31 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP RBL36L PA 66 LNP* LUBRICOMP* RBL36L is a compound based on Nylon 66 containing 30% Glass Bead, 15% PTFE. Added features s of this grade are: Low Extractable, Wear Resistant. |
|||
Izod Impact, Unnotched | 3.37 J/cm | 6.31 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP ZX07421 PPO LN:* LUBRICOMP* ZX07421 is a compound based on PPO resin containing proprietary fillers. Added feature of this grade is: Wear Resistant. |
|||
Izod Impact, Unnotched | 3.37 J/cm @Temperature 23.0 °C |
6.31 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp FF004 PE LNP THERMOCOMP* FF004 is a compound based on Polyethylene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 3.37 J/cm | 6.31 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP WX05502 Polyester Elastomer LNP THERMOCOMP* WX05502 is a compound based on Polyester, TP resin containing Flame Retardant, Glass Fiber, Mineral. Added features of this material include: Flame Retardant. |