Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 3.31 J/cm | 6.20 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® JK2000 PC+ABS (Asia Pacific) Lexan* JK2000 compound is a glass reinforced, non-Br and non-Cl FR polycarbonate blends designed for thinwall molding applications. |
|||
Izod Impact, Unnotched | 3.31 J/cm | 6.20 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP RL0019 PA 66 LNP LUBRICOMP* RL0019 is a compound based on Nylon 66 resin containing 5% PTFE. Added features of this material include: Flame Retardant, Wear Resistant. |
|||
Izod Impact, Unnotched | 3.31 J/cm | 6.20 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_JK2000 PC+ABS LNP* Thermocomp* Lexan_JK2000 compound is a 22% GR, ECO-compliant FR, PC+ABS for thinwall molding applications. |
|||
Izod Impact, Unnotched | 3.31 J/cm | 6.20 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_PCN2910 PPE+PS LNP* Thermodcomp* Noryl_PCN2910 compound is a 35% Glass/Mica filled. High modulus and tight tolerance molding for the chassis market. |
|||
Izod Impact, Unnotched | 3.31 J/cm | 6.20 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics NORYL PCN2910 PPE+PS (Asia Pacific) 35% Glass/Mica filled. High modulus and tight tolerance molding for the chassis market. |
|||
Izod Impact, Unnotched | 3.31 J/cm | 6.20 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP JX91198 PES LNP LUBRICOMP* JX91198 is a compound based on Polyethersulfone resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant. |
|||
Izod Impact, Unnotched | 3.31 J/cm | 6.20 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_PCN2910 PPE+PS (Asia Pacific) 35% Glass/Mica filled. High modulus and tight tolerance molding for the chassis market. |
|||
Izod Impact, Unnotched | 3.31 J/cm @Thickness 3.18 mm |
6.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Lubricomp® PDX-J-91198 Polyethersulfone, Proprietary Filler
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |