Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 25.63 J/cm | 48.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP 9X04488 POLYPHENYLENESULFONE (Asia Pacific) LNP* Thermocomp* 9X04488 is a compound based on POLYPHENYLENESULFONE resin containing Mineral. |
|||
Izod Impact, Unnotched | 25.63 J/cm | 48.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP 9X04488 PPS LNP* THERMOCOMP* 9X04488 is a compound based on PPS resin containing Mineral. |
|||
Izod Impact, Unnotched | 25.63 J/cm @Temperature 23.0 °C |
48.02 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp 9X04488 POLYPHENYLENESULFONE LNP* Thermocomp* 9X04488 is a compound based on POLYPHENYLENESULFONE resin containing Mineral.This data was supplied by SABIC-IP for the Americas region. |