Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 24.88 J/cm | 46.61 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP DL002ER PC LNP* Lubricomp* DL002ER is a compound based on Polycarbonate resin containing 10% PTFE. Added features of this material include: Internally Lubricated, Easy Molding, Mold Release. |
|||
Izod Impact, Unnotched | 24.88 J/cm | 46.61 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP DL002ER PC (Asia Pacific) LNP* Lubricomp* DL002ER is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Internally Lubricated, Easy Molding, Mold Release. |