Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 2.75 J/cm @Temperature -30.0 °C |
5.15 ft-lb/in @Temperature -22.0 °F |
ASTM D4812 |
SABIC Innovative Plastics Valox® DR48 PBT (Europe-Africa-Middle East) VALOX DR48 is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromoto.. |
|||
Izod Impact, Unnotched | 2.75 J/cm @Thickness 3.20 mm |
5.15 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Supreme Petrochem SP 246 Toughened Polystyrene Characteristics Excellent clarity Very high toughness Deep drawability Improved thermal stabilityProcessing Extrusion ThermoformingApplications Thermoformed clear and deep draw products Rectangu.. |
|||
Izod Impact, Unnotched | 2.75 J/cm @Thickness 3.20 mm |
5.15 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Supreme Petrochem SP 256 Toughened Polystyrene Characteristics Superior flexibility Good ball drop strength Excellent clarity Easy flow Processing Injection moldingApplications Transparent hangers Stationery items like pen barrels, geometric .. |
|||
Izod Impact, Unnotched | 2.75 J/cm @Thickness 3.20 mm |
5.15 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Supreme Petrochem SP EXP 31 Toughened Polystyrene Characteristics Very high clarity & gloss High dart impact strength & good stiffness Good crease retention Good heat resistance High yield compared to PVC, APET Processing Extrusion Vacuum form.. |