Polymer Property : Izod Impact, Unnotched = 2.51 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 2.51 - 13.3 J/cm
4.70 - 25.0 ft-lb/in
Average value: 4.72 J/cm Grade Count:12
Overview of materials for Polypropylene with 30% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are..
Izod Impact, Unnotched 2.51 J/cm

@Thickness 3.18 mm
4.70 ft-lb/in

@Thickness 0.125 in
ASTM D256
LNP Lubricomp® IBL-4416 Polyamide 6/12 Copolymer, Glass Bead Reinforced, Silicone Lubricant  (discontinued **)
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..