Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 2.40 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
4.50 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256 |
PolyOne Gravi-Tech™ GRV-NY-112-W-NAT Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Izod Impact, Unnotched | 2.40 J/cm | 4.50 ft-lb/in | ASTM D256 |
Network Polymers NPP 30-1200 TF40 Description: 40% Talc Filled Homopolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Izod Impact, Unnotched | 2.40 J/cm | 4.50 ft-lb/in | ASTM D256 |
Network Polymers NPP 30-2000 TF40 Description: 40% Talc Filled Homopolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Izod Impact, Unnotched | 2.40 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
4.50 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® 12-032
(discontinued **) PRE-ELEC 12-032 is a conductive thermoplastic compound based on a polyacetal copolymer with 20% carbon fiber. PRE-ELEC 12-032 exhibits excellent mechanical properties and electrical conductivity. Te.. |
|||
Izod Impact, Unnotched | 2.40 - 5340 J/cm | 4.50 - 10000 ft-lb/in | Average value: 6.94 J/cm Grade Count:13 |
Overview of materials for Polycarbonate, Conductive This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Conductive". Each property range of values reported is minimum and maximum values of appr.. |
|||
Izod Impact, Unnotched | 2.40 - 2.80 J/cm @Temperature 23.0 °C |
4.50 - 5.25 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RH 325 Rigid PVC, Antishock Extrusion Antishock furniture profiles |
|||
Izod Impact, Unnotched | 2.40 J/cm @Temperature 23.0 °C |
4.50 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Noryl TN240 PPE+PS PPE+PS blend. Unfilled. Transparent. Good flow. Scratch resistant. Injection molding. Suitable for housewares, personal care and small appliance applications.This data was supplied by SABIC-IP for t.. |
|||
Izod Impact, Unnotched | 2.40 J/cm @Thickness 3.17 mm |
4.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Electrablend® ABS 03008 Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: ESD ProtectionInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 2.40 J/cm @Thickness 3.17 mm |
4.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Electrablend® ABS 03009 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: Conductive, Electromagnetic Shielding (EMI) and Radio Frequency Shielding (RFI)Information provided.. |
|||
Izod Impact, Unnotched | 2.40 J/cm @Thickness 3.17 mm |
4.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Electrablend® ABS 03010 Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: ESD Protection and Good MoldabilityInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 2.40 J/cm @Thickness 3.17 mm |
4.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Electrablend® HDPE 04001 LE BK Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: ESD Protection and ConductiveAppearance: BlackProcessing Method: ExtrusionInformation provided by .. |
|||
Izod Impact, Unnotched | 2.40 J/cm | 4.50 ft-lb/in | ASTM D256 |
Spartech SolarKote® /ABS Weatherable Sheet Description: Weatherable SheetSolarKote is a registered trademark of Atofina Chemicals, Inc..Information provided by Spartech. |
|||
Izod Impact, Unnotched | 2.40 J/cm @Thickness 3.17 mm |
4.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Electrablend® ABS SS15 BK MB 15% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 15% Filler by WeightFeatures: Electromagnetic Shielding (EMI)Appearance: BlackInformation provided by TP Composi.. |
|||
Izod Impact, Unnotched | 2.40 J/cm @Thickness 3.17 mm |
4.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Electrablend® ABS SS7 BK MB 7% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 7% Filler by WeightFeatures: ESD ProtectionAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 2.40 J/cm | 4.50 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP IF003 PA 6/12 LNP THERMOCOMP* IF003 is a compound based on Nylon 6/12 resin containing 15% Glass Fiber. |
|||
Izod Impact, Unnotched | 2.40 J/cm @Thickness 3.17 mm |
4.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Luriblend® POM HO TL20 Acetal Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%)Features: Lubricated and HomopolymerInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 2.40 J/cm | 4.50 ft-lb/in | At 73°F; ASTM D256 |
Plastics Group Polifil® T-40 40% Talc-Reinforced Polypropylene Polifil® T series compounds are homopolymer polypropylene resins reinforced with asbestos-free talc. They possess high flex modulus, high deflection temperature, good chemical resistance and colora.. |
|||
Izod Impact, Unnotched | 2.40 J/cm | 4.50 ft-lb/in | ASTM D256 |
Adell EQ-16 Homopolymer Polypropylene, 30% Mica Filled Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Unnotched | 2.40 - 16.0 J/cm | 4.50 - 30.0 ft-lb/in | Average value: 6.99 J/cm Grade Count:10 |
Overview of materials for Polypropylene with 10% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Talc Filler". Specific grades with primary filler content between 5% and 14% are .. |