Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 2.02 J/cm | 3.78 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP AL003 ABS LNP LUBRICOMP* AL003 is a compound based on Acrylonitrile Butadiene Styrene resin containing 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 2.02 J/cm | 3.78 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP AL003 ABS (Europe-Africa-Middle East) LNP LUBRICOMP* AL003 is a compound based on Acrylonitrile Butadiene Styrene resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 2.02 J/cm | 3.78 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP AL003 ABS (Asia Pacific) LNP LUBRICOMP* AL003 is a compound based on Acrylonitrile Butadiene Styrene resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 2.02 J/cm | 3.78 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP HH0420A PA11 LNP* HH0420A is a compound based on Nylon 11 containing proprietary fillers. Added features of this material are High Specific Gravity. |
|||
Izod Impact, Unnotched | 2.02 J/cm | 3.78 ft-lb/in | 63.5*12.7*3.2mm, Cut; ASTM D4812 |
SABIC Innovative Plastics SABIC PPCOMPOUND 19T1040 PP SABIC® PPcompound 19T1040 is a general purpose, talc filled, heat stabilized homopolymer polypropylene compound. This compound exhibits high flow and is suitable for injection molding application.. |
|||
Izod Impact, Unnotched | 2.02 J/cm | 3.78 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP 5C003 FP-V (PVDF) LNP THERMOCOMP* 5C003 is a compound based on Polyvinylidene Fluoride resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched | 2.02 J/cm | 3.78 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP HH0420A PA11 LNP* THERMOCOMP* HH0420A is a compound based on Nylon 11 containing proprietary fillers. Added features of this material are High Specific Gravity. |
|||
Izod Impact, Unnotched | 2.02 J/cm @Temperature 23.0 °C |
3.78 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp 5C003 LNP THERMOCOMP* 5C003 is a compound based on Polyvinylidene Fluoride resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. Also known as THERMOCOMP* FP-VC.. |
|||
Izod Impact, Unnotched | 2.02 J/cm @Thickness 6.40 mm |
3.78 ft-lb/in @Thickness 0.252 in |
ASTM D4812 |
SABIC Innovative Plastics NORYL FN215X PPE+PS Structural foam resin. 170F (77C) HDT. Improved reliability and productivity. All values at 20% weight reduction. |