Izod Impact, Unnotched 15.85 J/cm
29.69 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP RF00AS PA 66
LNP THERMOCOMP* RF00AS is a compound based on Nylon 66 resin containing 50% Glass Fiber. Added features of this material include: Heat Stabilized.