Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 11.17 J/cm | 20.93 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP RX98372H PA 66 (Asia Pacific) LNP* Thermocomp* RX98372H is a compound based on Nylon 66 resin containing Glass Fiber. |