Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | >= 10.7 J/cm | >= 20.0 ft-lb/in | ASTM D256 |
Network Polymers Kepital® F20-03 Description: Natural Acetal CopolymerInformation provided by Network Polymers Inc. |
|||
Izod Impact, Unnotched | >= 10.7 J/cm | >= 20.0 ft-lb/in | ASTM D256 |
Network Polymers Kepital® F30-03 Description: Natural Acetal CopolymerInformation provided by Network Polymers Inc. |
|||
Izod Impact, Unnotched | 10.7 - 5340 J/cm | 20.0 - 10000 ft-lb/in | Average value: 21.9 J/cm Grade Count:19 |
Overview of materials for Nylon 66, 60% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. .. |
|||
Izod Impact, Unnotched | 10.7 J/cm @Thickness 3.17 mm |
20.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 GF50 X BK 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAppearance: BlackTPCI# 6560101Information provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 10.7 J/cm @Thickness 3.17 mm |
20.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Luriblend® PC TL15 Availability: North AmericaForms: PelletsAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 10.7 J/cm | 20.0 ft-lb/in | ASTM D4812 |
A. Schulman SCHULAMID® 66 GF40H 40% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 10.7 - 42.7 J/cm | 20.0 - 80.0 ft-lb/in | ASTM D256 |
Arkema Group KYNAR® 710, 710 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |
|||
Izod Impact, Unnotched | 10.7 J/cm | 20.0 ft-lb/in | ASTM D4812 |
Asahi Kasei Thermylon® NSG-440A 60% Ceramic and Glass Fiber Reinforced Information provided by Asahi Thermofil |