Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 1.87 - 8.81 J/cm | 3.50 - 16.5 ft-lb/in | Average value: 5.96 J/cm Grade Count:6 |
Overview of materials for Acetal Copolymer, Steel Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Steel Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Unnotched | 1.87 - 6.14 J/cm | 3.50 - 11.5 ft-lb/in | Average value: 3.36 J/cm Grade Count:19 |
Overview of materials for Polycarbonate, NCG Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, NCG Filled". Each property range of values reported is minimum and maximum values of appr.. |
|||
Izod Impact, Unnotched | 1.87 J/cm @Thickness 3.17 mm |
3.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Plastiblend® PPS/F 0328 Availability: North AmericaForms: Pellets Additive: Lubricant and Strontium Ferrite Features: LubricatedInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 1.87 J/cm @Thickness 3.17 mm |
3.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Electrafil® J-1200/CF/10 ABS, 10% Carbon Fiber Reinforced |
|||
Izod Impact, Unnotched | 1.87 J/cm | 3.50 ft-lb/in | ASTM D256 |
Westlake Plastics Absylux® CN-F Acrylonitrile-Butadiene-Styrene (conductive) Non-sloughing, carbon-fiber-filled material with high strength and stiffness; easily machined.Information provided by Westlake Plastics. |
|||
Izod Impact, Unnotched | 1.87 J/cm | 3.50 ft-lb/in | ASTM D256 |
Westlake Plastics Pomalux® CN-F Acetal Copolymer (conductive) Non-sloughing carbon-fiber-filled material which is extremely strong and stiff with excellent dimensional stability. Abrasion-resistant, highly chemical-resistant, with temperature resistance to 32.. |
|||
Izod Impact, Unnotched | 1.87 - 5340 J/cm | 3.50 - 10000 ft-lb/in | Average value: 6.03 J/cm Grade Count:136 |
Overview of materials for Polyethersulfone (PES) This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Izod Impact, Unnotched | 1.87 - 7.47 J/cm | 3.50 - 14.0 ft-lb/in | Average value: 5.99 J/cm Grade Count:16 |
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Izod Impact, Unnotched | 1.87 - 10.7 J/cm | 3.50 - 20.0 ft-lb/in | Average value: 4.43 J/cm Grade Count:13 |
Overview of materials for Polypropylene Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Glass Bead Filled". Each property range of values reported is minimum and maximum values o.. |