Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 1.655 J/cm | 3.100 ft-lb/in | ASTM D256 |
Stratasys® Polyphenylsulfone PPSF/PPSU (polyphenylsulfone) material has the greatest strength, heat and chemical resistance of all Stratasys materials - ideal for aerospace, automotive and medical applications. Stratasys FDM (F.. |
|||
Izod Impact, Unnotched | 1.655 J/cm | 3.100 ft-lb/in | ASTM D256 |
Proto3000 PPSF Fused Deposition Modeling Polymer Description: PPSF/PPSU (polyphenylsulfone) material has the greatest heat and chemical resistance of all Fortus materials - ideal for aerospace, automotive and medical applications. PPSF parts manuf.. |