Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 1.17 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Niche Polymer PA66GI14BK Nylon 66, 14% Glass Fiber Filled, Impact Modified Information provided by Niche Polymer |
|||
Izod Impact, Unnotched | 1.17 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Niche Polymer PPCG30BK Copolymer PP, 30% Glass Fiber Filled Information provided by Niche Polymer |
|||
Izod Impact, Unnotched | 1.17 J/cm | 2.19 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP CZL36 PS LNP LUBRICOMP* CZL36 is a compound based on Polystyrene resin containing 30% Milled Glass and 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 1.17 - 13.3 J/cm | 2.20 - 25.0 ft-lb/in | Average value: 5.86 J/cm Grade Count:31 |
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum.. |