Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 0.641 J/cm - NB | 1.20 ft-lb/in - NB | Average value: 0.641 J/cm Grade Count:6 |
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i.. |
|||
Izod Impact, Unnotched | 0.641 J/cm | 1.20 ft-lb/in | |
Wingate Alloys Winco Poly NLT Engineered UHMW Winco Poly NLT is one of the oldest and most widely used engineered mechanical plastics. Its combination of toughness, dimensional stability, wear resistance, availability and versatility make it a .. |