Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Creep Strength | 32.0 MPa @Time 36000 sec |
4640 psi @Time 10.0 hour |
in water at 95°C |
BASF Ultrason S 3010 PSU Ultrason S 3010 is an unreinforced, higher viscosity injection molding and extrusion PSU grade, tougher and with improved chemical resistance. It conforms to FDA requirements of 21 CFR 177.1655. |