Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Creep Strength | 21.0 MPa @Temperature 899 °C |
3050 psi @Temperature 1650 °F |
0.0001% per hour |
ATI Allegheny Ludlum Altemp® HX Nickel-Based superalloy Characteristics: outstanding resistance to oxidation at high temperatures, exceptional strength at elevated temperatures, good fabricability, good machinability in annealed condition, work hardening.. |