Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Creep Strength | 96.5 MPa @Temperature 204 °C, Time 360000 sec |
14000 psi @Temperature 400 °F, Time 100 hour |
0.1% creep strain |
Magnesium Elektron Elektron® 21 Magnesium Casting Alloy Fully heat treatable alloy for use up to 400°F. Excellent corrosion resistance and castability. Cast products possess a fine-grained microstructure and pressure tightness. Easily machined. Usual .. |