Polymer Property : Creep Strength = 43.5 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Creep Strength 0.0600 - 0.300 MPa
8.70 - 43.5 psi
Average value: 0.156 MPa Grade Count:6
Overview of materials for Expanded Polystyrene (EPS)
This property data is a summary of similar materials in the MatWeb database for the category "Expanded Polystyrene (EPS)". Each property range of values reported is minimum and maximum values of app..
Creep Strength 0.0600 - 0.300 MPa
8.70 - 43.5 psi
Average value: 0.156 MPa Grade Count:6
Overview of materials for Polystyrene, Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a..