Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Creep Strength | 0.0600 - 0.300 MPa | 8.70 - 43.5 psi | Average value: 0.156 MPa Grade Count:6 |
Overview of materials for Expanded Polystyrene (EPS) This property data is a summary of similar materials in the MatWeb database for the category "Expanded Polystyrene (EPS)". Each property range of values reported is minimum and maximum values of app.. |
|||
Creep Strength | 0.0600 - 0.300 MPa | 8.70 - 43.5 psi | Average value: 0.156 MPa Grade Count:6 |
Overview of materials for Polystyrene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a.. |