Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Crush Resistance | 3630 kg | 8000 lb (mass) | Compressive Strength |
Glastic Laminates/Shapes 2165 Fiberglass-Reinforced Polyester Standoff Insulator Data provided by Glastic Corporation.Molded from UL recognized molding compound. Moisture and heat resistance of Glastic Insulators are higher than those of conventional plastic insulators. |