Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Crush Resistance | 27200 kg | 60000 lb (mass) | Compressive Strength |
Glastic Laminates/Shapes 1461 Fiberglass-Reinforced Polyester Standoff Insulator Data provided by Glastic Corporation.Molded from UL recognized molding compound. Moisture and heat resistance of Glastic Insulators are higher than those of conventional plastic insulators. |