| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Charpy Impact Unnotched | 2.90 J/cm² @Temperature -30.0 °C |
13.8 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
| Nilit FRIANYL A63 CV-CM 0515 9005/Z Powder-coatable nylon 6.6 for injection molding, 15% ceramic filled Powder-coatable nylon 6.6 for injection molding, with conductive carbon blackInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
| Charpy Impact Unnotched | 2.90 J/cm² @Temperature -30.0 °C |
13.8 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
| Nilit FRIANYL A63 HH-FK 1020 Nylon 6.6 for injection molding, 10% glass fiber and 20% glass ball reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
| Charpy Impact Unnotched | 2.90 J/cm² @Temperature -40.0 °C |
13.8 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
| Nilit FRIANYL A63 W-GV20 Nylon 6.6 for injection molding, 20% glass fiber reinforced Nylon 6.6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
| Charpy Impact Unnotched | 2.90 J/cm² | 13.8 ft-lb/in² | ISO 179/1eU |
| Nilit FRIANYL A63 V0 G5 Nylon 6.6 for injection molding, 25% glass fiber reinforced Nylon 6.6 for injection molding, flame retardant, free of halogen and phosphorus.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
| Charpy Impact Unnotched | 2.91 J/cm² | 13.8 ft-lb/in² | ISO 179/1eU |
| NOVA Chemicals Dylark® 510XT Glass Reinforced Engineering Resin Features: Higher toughness product, Excellent stiffness, High heat resistance, Superior adhesion to urethane foamApplications: Instrument panel substrates, Mid-Consoles, Center Stacks, Interior tri.. |
|||
| Charpy Impact Unnotched | 2.90 - 999.9 J/cm² @Temperature -20.0 - -20.0 °C |
13.8 - 4759 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Average value: 7.04 J/cm² Grade Count:18 |
| Overview of materials for Polypropylene with 20% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Mica Filler". Specific grades with primary filler content between 15% and 24% are.. |
|||
| Charpy Impact Unnotched | 2.90 J/cm² | 13.8 ft-lb/in² | |
| Idemitsu Kosan Xarec® EA 543 SPS, 40% Glass Filled |
|||
| Charpy Impact Unnotched | 2.90 J/cm² | 13.8 ft-lb/in² | flatwise; ISO 179 1fU |
| Lehmann & Voss LUVOCOM® NY-4/PL/15/BK Polyamide 612, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
| Charpy Impact Unnotched | 2.90 J/cm² | 13.8 ft-lb/in² | ISO 179/2C |
| SABIC Innovative Plastics Valox® 771 PBT (Europe-Africa-Middle East) VALOX 771 is a 15% glass and 20% mineral filled, flame retarded injection moulding PBT resin. |
|||
| Charpy Impact Unnotched | 2.90 J/cm² @Temperature -30.0 °C |
13.8 ft-lb/in² @Temperature -22.0 °F |
ISO 179/2C |
| SABIC Innovative Plastics Valox® 771 PBT (Europe-Africa-Middle East) VALOX 771 is a 15% glass and 20% mineral filled, flame retarded injection moulding PBT resin. |
|||
| Charpy Impact Unnotched | 2.90 J/cm² | 13.8 ft-lb/in² | ISO 179/2C |
| SABIC Innovative Plastics Valox® SHF4930 PBT (Europe-Africa-Middle East) Super high flow FR PBT grade with 15% Glass reinforced |
|||
| Charpy Impact Unnotched | 2.90 J/cm² | 13.8 ft-lb/in² | ISO 179 |
| Chi Mei Kibiton® PB-5910 SBC High transparency, medium stiffness, toughness |
|||
| Charpy Impact Unnotched | 2.90 J/cm² | 13.8 ft-lb/in² | ISO 179/IeU |
| Addiplast Addilene H 526 N30 Polypropylene Homopolymer Improved rigidity, high durabilityInformation provided by Addiplast. |
|||
| Charpy Impact Unnotched | 2.90 J/cm² | 13.8 ft-lb/in² | ISO 179/1eU |
| Solvay Specialty Polymers Amodel® A-1240 L Polyphthalamide (PPA)
(discontinued **) Amodel A-1240 L is a 40% mineral filled polyphthalamide (PPA) that offers low warpage and excellent dimensional stability. This resin also has a high deflection temperature, flexural modulus and ten.. |
|||