Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 1.30 - 1.50 J/cm² | 6.19 - 7.14 ft-lb/in² | ISO 11542-2 |
Okulen® 1000 - REG PE Colored OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
Charpy Impact Unnotched | 1.00 - 1.50 J/cm² | 4.76 - 7.14 ft-lb/in² | ISO 11542-2 |
Okulen® 500 - REG PE Multicoloured coarse OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel.. |
|||
Charpy Impact Unnotched | 1.00 - 1.50 J/cm² | 4.76 - 7.14 ft-lb/in² | ISO 11542-2 |
Okulen® 500 - REG PE Multicoloured fine OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel.. |
|||
Charpy Impact Unnotched | 0.200 - 1.50 J/cm² | 0.952 - 7.14 ft-lb/in² | Average value: 0.730 J/cm² Grade Count:9 |
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled". Each property range of values repor.. |
|||
Charpy Impact Unnotched | 0.400 - 1.50 J/cm² | 1.90 - 7.14 ft-lb/in² | Average value: 0.928 J/cm² Grade Count:10 |
Overview of materials for Phenolic, Novolac, Mineral/Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Glass Filled". Each property range of values reported is minimum and maximum .. |
|||
Charpy Impact Unnotched | 1.50 - 1.50 J/cm² @Temperature -20.0 - -20.0 °C |
7.14 - 7.14 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Average value: 1.50 J/cm² Grade Count:1 |
Overview of materials for Nylon 6, Mineral Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Mineral Reinforced, Impact Grade". Each property range of values reported is minimum and maximu.. |
|||
Charpy Impact Unnotched | 1.30 - 1.50 J/cm² | 6.19 - 7.14 ft-lb/in² | ISO 179 |
Vyncolit 2950 W Novolac Phenolic Mineral and glass fiber filled phenolic molding compound with a very high strain to failure in flexure. UL listed.USES: Armature insulation.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Charpy Impact Unnotched | 1.00 - 1.50 J/cm² | 4.76 - 7.14 ft-lb/in² | Compression; ISO 179/1eU |
Raschig Group RALUPOL® 8605 UP Polyester Glass fiber reinforced polyester molding compound. Resistant to hydrolysis. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU dire.. |