Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 7.50 - 11.0 J/cm² | 35.7 - 52.4 ft-lb/in² | Average value: 9.17 J/cm² Grade Count:39 |
Overview of materials for Nylon 610, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap.. |
|||
Charpy Impact Unnotched | 6.00 - 11.0 J/cm² @Temperature -30.0 - 30.0 °C |
28.6 - 52.4 ft-lb/in² @Temperature -22.0 - 86.0 °F |
Average value: 8.87 J/cm² Grade Count:24 |
Overview of materials for Nylon 610, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap.. |
|||
Charpy Impact Unnotched | 2.00 - 11.0 J/cm² @Temperature -30.0 - 30.0 °C |
9.52 - 52.4 ft-lb/in² @Temperature -22.0 - 86.0 °F |
Average value: 7.73 J/cm² Grade Count:19 |
Overview of materials for Nylon 612, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of .. |
|||
Charpy Impact Unnotched | 2.50 - 11.0 J/cm² | 11.9 - 52.4 ft-lb/in² | Average value: 8.05 J/cm² Grade Count:47 |
Overview of materials for Nylon 46, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values .. |
|||
Charpy Impact Unnotched | 1.00 - 11.0 J/cm² @Temperature -30.0 - -30.0 °C |
4.76 - 52.4 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 6.00 J/cm² Grade Count:2 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum.. |