Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 0.700 - 1000 J/cm² | 3.33 - 4760 ft-lb/in² | Average value: 2.38 J/cm² Grade Count:25 |
Overview of materials for Polystyrene, Molded, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Charpy Impact Unnotched | 1.50 - 1000 J/cm² | 7.14 - 4760 ft-lb/in² | Average value: 2.42 J/cm² Grade Count:24 |
Overview of materials for Acetal Copolymer, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
Charpy Impact Unnotched | 13.0 - 1000 J/cm² | 61.9 - 4760 ft-lb/in² | Average value: 16.3 J/cm² Grade Count:29 |
Overview of materials for Acetal Homopolymer, Unreinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced, Impact Grade". Each property range of values reported is minimum and m.. |
|||
Charpy Impact Unnotched | 3.50 - 1000 J/cm² | 16.7 - 4760 ft-lb/in² | Average value: 4.50 J/cm² Grade Count:7 |
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a.. |
|||
Charpy Impact Unnotched | 1.50 - 1000 J/cm² | 7.14 - 4760 ft-lb/in² | Average value: 1.50 J/cm² Grade Count:3 |
Overview of materials for PVC, Extruded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Extruded". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Charpy Impact Unnotched | 3.80 - 1000 J/cm² | 18.1 - 4760 ft-lb/in² | Average value: 4.90 J/cm² Grade Count:6 |
Overview of materials for Polypropylene, Mineral Reinforced, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced, Impact Modified". Each property range of values reported is minimum a.. |
|||
Charpy Impact Unnotched | 6.30 - 1000 J/cm² | 30.0 - 4760 ft-lb/in² | Average value: 12.6 J/cm² Grade Count:18 |
Overview of materials for Polypropylene with 20% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Mica Filler". Specific grades with primary filler content between 15% and 24% are.. |
|||
Charpy Impact Unnotched | 5.00 - 1000 J/cm² | 23.8 - 4760 ft-lb/in² | Average value: 5.50 J/cm² Grade Count:3 |
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be.. |
|||
Charpy Impact Unnotched | 1.50 - 1000 J/cm² | 7.14 - 4760 ft-lb/in² | Average value: 4.78 J/cm² Grade Count:77 |
Overview of materials for Nylon 6, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
Charpy Impact Unnotched | 3.00 - 1000 J/cm² | 14.3 - 4760 ft-lb/in² | Average value: 8.87 J/cm² Grade Count:69 |
Overview of materials for Nylon 610 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Charpy Impact Unnotched | 10.0 - 1000 J/cm² | 47.6 - 4760 ft-lb/in² | Average value: 13.4 J/cm² Grade Count:9 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyester Grade". Each property range of values reported is minimum a.. |
|||
Charpy Impact Unnotched | 10.0 - 1000 J/cm² | 47.6 - 4760 ft-lb/in² | Average value: 15.4 J/cm² Grade Count:12 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced". Each property range of values reported is mi.. |
|||
Charpy Impact Unnotched | 4.20 - 1000 J/cm² | 20.0 - 4760 ft-lb/in² | Average value: 6.03 J/cm² Grade Count:17 |
Overview of materials for Polypropylene with 10% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Talc Filler". Specific grades with primary filler content between 5% and 14% are .. |
|||
Charpy Impact Unnotched | 1.70 - 1000 J/cm² | 8.09 - 4760 ft-lb/in² | Average value: 4.44 J/cm² Grade Count:23 |
Overview of materials for Polypropylene with 40% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are.. |
|||
Charpy Impact Unnotched | 1.50 - 1000 J/cm² | 7.14 - 4760 ft-lb/in² | Average value: 5.06 J/cm² Grade Count:10 |
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and.. |
|||
Charpy Impact Unnotched | 0.400 - 1000 J/cm² | 1.90 - 4760 ft-lb/in² | Average value: 0.975 J/cm² Grade Count:5 |
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Unreinforced, Extruded". Each property range of values reported is minimum .. |
|||
Charpy Impact Unnotched | 0.600 - 1000 J/cm² | 2.86 - 4760 ft-lb/in² | Average value: 3.37 J/cm² Grade Count:13 |
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and .. |
|||
Charpy Impact Unnotched | 0.500 - 1000 J/cm² | 2.38 - 4760 ft-lb/in² | Average value: 4.95 J/cm² Grade Count:70 |
Overview of materials for Polypropylene with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i.. |
|||
Charpy Impact Unnotched | 1.40 - 1000 J/cm² | 6.66 - 4760 ft-lb/in² | Average value: 1.40 J/cm² Grade Count:8 |
Overview of materials for Polypropylene with Carbon Black Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v.. |
|||
Charpy Impact Unnotched | 2.20 - 1000 J/cm² | 10.5 - 4760 ft-lb/in² | Average value: 4.15 J/cm² Grade Count:7 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported.. |