Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 0.450 - 10.0 J/cm² | 2.14 - 47.6 ft-lb/in² | Average value: 4.31 J/cm² Grade Count:101 |
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15.. |
|||
Charpy Impact Unnotched | 2.50 - 10.0 J/cm² | 11.9 - 47.6 ft-lb/in² | Average value: 5.53 J/cm² Grade Count:4 |
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled". Specific grades with glass content between 15% an.. |
|||
Charpy Impact Unnotched | 1.50 - 10.0 J/cm² | 7.14 - 47.6 ft-lb/in² | Average value: 5.14 J/cm² Grade Count:58 |
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Charpy Impact Unnotched | 9.17 - 10.0 J/cm² @Temperature -30.0 - -30.0 °C |
43.6 - 47.6 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 9.59 J/cm² Grade Count:2 |
Overview of materials for Nylon 11 with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are includ.. |
|||
Charpy Impact Unnotched | 4.50 - 10.0 J/cm² | 21.4 - 47.6 ft-lb/in² | Average value: 7.98 J/cm² Grade Count:20 |
Overview of materials for Nylon 12, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Charpy Impact Unnotched | 4.00 - 10.0 J/cm² @Temperature -30.0 - 30.0 °C |
19.0 - 47.6 ft-lb/in² @Temperature -22.0 - 86.0 °F |
Average value: 7.89 J/cm² Grade Count:18 |
Overview of materials for Nylon 12, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Charpy Impact Unnotched | 6.00 - 10.0 J/cm² | 28.6 - 47.6 ft-lb/in² | Average value: 8.00 J/cm² Grade Count:21 |
Overview of materials for Nylon 12, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. .. |
|||
Charpy Impact Unnotched | 4.00 - 10.0 J/cm² @Temperature -30.0 - -30.0 °C |
19.0 - 47.6 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 6.87 J/cm² Grade Count:42 |
Overview of materials for Nylon 46, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values .. |
|||
Charpy Impact Unnotched | 5.00 - 10.0 J/cm² | 23.8 - 47.6 ft-lb/in² | Average value: 7.06 J/cm² Grade Count:8 |
Overview of materials for Polystyrene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a.. |