Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 4.70 - 7.00 J/cm² | 22.4 - 33.3 ft-lb/in² | Average value: 5.88 J/cm² Grade Count:5 |
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35.. |
|||
Charpy Impact Unnotched | 2.20 - 7.00 J/cm² | 10.5 - 33.3 ft-lb/in² | Average value: 5.51 J/cm² Grade Count:17 |
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45.. |
|||
Charpy Impact Unnotched | 2.00 - 7.00 J/cm² | 9.52 - 33.3 ft-lb/in² | Average value: 4.04 J/cm² Grade Count:13 |
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar.. |
|||
Charpy Impact Unnotched | 2.50 - 7.00 J/cm² @Temperature -40.0 - 30.0 °C |
11.9 - 33.3 ft-lb/in² @Temperature -40.0 - 86.0 °F |
Average value: 4.64 J/cm² Grade Count:11 |
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are incl.. |
|||
Charpy Impact Unnotched | 3.50 - 7.00 J/cm² | 16.7 - 33.3 ft-lb/in² | Average value: 5.62 J/cm² Grade Count:13 |
Overview of materials for Nylon 12, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Charpy Impact Unnotched | 3.00 - 7.00 J/cm² @Temperature -20.0 - 30.0 °C |
14.3 - 33.3 ft-lb/in² @Temperature -4.00 - 86.0 °F |
Average value: 4.40 J/cm² Grade Count:5 |
Overview of materials for Nylon 66/6, Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, Mineral Reinforced". Each property range of values reported is minimum and maximum values of.. |
|||
Charpy Impact Unnotched | 2.30 - 7.00 J/cm² | 10.9 - 33.3 ft-lb/in² | Average value: 4.54 J/cm² Grade Count:41 |
Overview of materials for PBT + PET Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Charpy Impact Unnotched | 2.00 - 7.00 J/cm² @Temperature -30.0 - -30.0 °C |
9.52 - 33.3 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 4.27 J/cm² Grade Count:34 |
Overview of materials for PBT + PET Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Charpy Impact Unnotched | 2.70 - 7.00 J/cm² | 12.8 - 33.3 ft-lb/in² | Average value: 4.88 J/cm² Grade Count:13 |
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% .. |
|||
Charpy Impact Unnotched | 2.30 - 7.00 J/cm² | 10.9 - 33.3 ft-lb/in² | Average value: 4.49 J/cm² Grade Count:27 |
Overview of materials for Polypropylene with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i.. |