Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 0.600 - 0.800 J/cm² @Temperature 23.0 °C |
2.86 - 3.81 ft-lb/in² @Temperature 73.4 °F |
Injection and Compression; ISO 179/ 1eU |
Raschig Group 3536 Epoxy Glass-fiber reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. This product meets the allowed.. |
|||
Charpy Impact Unnotched | 0.500 - 0.800 J/cm² | 2.38 - 3.81 ft-lb/in² | Compression; ISO 179/1eU |
Raschig Group RALUPOL® 2100 UP Polyester Organically and inorganically filled polyester molding compound. Low post-shrinkage, very good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy meta.. |
|||
Charpy Impact Unnotched | 0.600 - 0.800 J/cm² | 2.86 - 3.81 ft-lb/in² | ISO 179 |
Vyncolit 2530 W Novolac Phenolic Mineral and organic filled phenolic molding compound with excellent thermal properties.USES: Lamp sockets, special lamp holders, pan handles and knobs.Information provided by Vyncolit, a Sumitomo Ba.. |
|||
Charpy Impact Unnotched | 0.650 - 0.800 J/cm² | 3.09 - 3.81 ft-lb/in² | ISO 179 |
Vyncolit 2920 W Novolac Phenolic Mineral and organic filled molding compound with good dimensional stability and heat resistance.USES: Carburettor and intake manifold thermal insulator.Information provided by Vyncolit, a Sumitomo B.. |
|||
Charpy Impact Unnotched | 0.600 - 0.800 J/cm² | 2.86 - 3.81 ft-lb/in² | Compression; ISO 179/1eU |
Raschig Group RESINOL® 400 EPF Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets .. |
|||
Charpy Impact Unnotched | 0.650 - 0.800 J/cm² @Temperature 23.0 °C |
3.09 - 3.81 ft-lb/in² @Temperature 73.4 °F |
Injection; ISO 179/ 1eU |
Raschig Group 5557 DAP
(discontinued **) Glass fiber-reinforced and inorganically filled diallylphthalate molding compound (DAP) in various colors. Good mechanical strength together with retention of high electrical properties under hot h.. |
|||
Charpy Impact Unnotched | 0.800 - 0.800 J/cm² @Temperature -20.0 - -20.0 °C |
3.81 - 3.81 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Average value: 0.800 J/cm² Grade Count:1 |
Overview of materials for Polypropylene with 40% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Mica Filler". Specific grades with primary filler content between 35% and 44% are.. |