Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 3.20 - 3.20 J/cm² @Temperature -20.0 - -20.0 °C |
15.2 - 15.2 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Average value: 3.20 J/cm² Grade Count:1 |
Overview of materials for Polycarbonate, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E.. |