Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 1.39 - 6.50 J/cm² @Temperature -40.0 - 30.0 °C |
6.62 - 30.9 ft-lb/in² @Temperature -40.0 - 86.0 °F |
Average value: 3.68 J/cm² Grade Count:66 |
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15.. |