Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 1.39 J/cm² | 6.61 ft-lb/in² | ISO 179-1 |
Vyncolit BXE7670 Glass Filled Phenolic Molding Compound Novolac resin based, mainly glass fiber filled. Due to its unique composition, excellent balance between mechanical, thermal and dimensional stability.Information provided by Sumitomo Bak North Ame.. |