Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 10.5 J/cm² | 50.0 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Cycoloy® CM8622 PC+ABS (Europe-Africa-Middle East) CYCOLOY* CM8622 is a high heat PC/ABS blend offering high modulus, low CTE and good |
|||
Charpy Impact Unnotched | 10.5 J/cm² | 50.0 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYL® A 218G2 V30 Black 34N PA66, 30% glass fiber, Conditioned Description: TECHNYL® A 218G2 V30 Black 34N is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color. Benefits: This .. |
|||
Charpy Impact Unnotched | 10.5 J/cm² | 50.0 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYL® C 218 V 30 PA6, 30% glass fiber, Conditioned Description: TECHNYL® C 218 V30 is a polyamide 6, heat stabilized, reinforced with 30% of glass fiber, for injection molding. This product is available in black color.Benefits: The product offers.. |
|||
Charpy Impact Unnotched | 10.5 J/cm² | 50.0 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYL® C 246 V 30 PA6, 30% glass fiber, Conditioned Description: Polyamide PA6, reinforced with 30 % of glass fiber, high impact strength, for injection molding.Available in: Asia Pacific and North AmericaProduct Applications: Having good mechanical .. |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature 23.0 °C |
50.0 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eU |
DSM Novamid® 1015G50 NA/BK37 PA6-GF50 50% Glass Reinforced, Injection Molding |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature 23.0 °C |
50.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6000 GV 20 HWCP 20% Glass Fiber Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature 23.0 °C |
50.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6000 GV 25 HWCP 25% Glass Fiber Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature 23.0 °C |
50.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6600 GV 40 HWCP 40% Glass Fiber Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature 23.0 °C |
50.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6600 GV 45 HWCP 45% Glass Fiber Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact Unnotched | 10.5 J/cm² | 50.0 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® GVL-5H black 9839 PA*-GF50 Product description: Grivory GVL-5H black 9839 is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long glass fibers. Grivory GVL-5H.. |
|||
Charpy Impact Unnotched | 10.5 J/cm² | 50.0 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® GVL-5H nat PA*-GF50 Product description: Grivory GVL-5H natural is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long glass fibers. Grivory GVL-5H na.. |
|||
Charpy Impact Unnotched | 10.5 J/cm² | 50.0 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® TSGL-50-4 black 9839 PA666-GF50 Product description: Grilon TSGL-50/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 50% long glass fibers. Grilon TSGL-50/4 natural is characterized by the following .. |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature 30.0 °C |
50.0 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® TSGL-60/4 black 9839 PA666-GF60 Product description: Grilon TSGL-60/4 black 9839 is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 60% long glass fibers. Grilon TSGL-60/4 black 9839 is characterized by the foll.. |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature 30.0 °C |
50.0 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® TSGL-60/4 nat PA666-GF60 Product description: Grilon TSGL-60/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 60% long glass fibers. Grilon TSGL-60/4 natural is characterized by the following .. |
|||
Charpy Impact Unnotched | 10.5 J/cm² | 50.0 ft-lb/in² | DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® PLS 95G40DH1T BK261 Nylon 6
(Unverified Data**) 40% Glass Reinforced Heat Stabilized Polyamide Zytel PLS95G40DH1T is a 40% GR impact modified PA made with SHIELD technology its superior heatInformation provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 10.5 J/cm² | 50.0 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® GVL-6H black 9839 PA*-GF60 Product description: Grivory GVL-6H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long glass fibers. Grivory GVL-6H blac.. |
|||
Charpy Impact Unnotched | 10.5 J/cm² | 50.0 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® GVL-6H black 9915 PA*-GF60 Product description: Grivory GVL-6H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long glass fibers. Grivory GVL-6H blac.. |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature 23.0 °C |
50.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Akro-Plastic Akromid® A3 GF 60 (2424) PA 6.6 Conditioned, 60% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Charpy Impact Unnotched | 10.5 J/cm² | 50.0 ft-lb/in² | |
BASF Novolen® 1101 P Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 10.5 J/cm² | 50.0 ft-lb/in² | ISO 179/1eU |
BASF Ultramid® B3G8 BK00564 40% Glass Filled PA6 (Conditioned) Ultramid B3G8 BK00564 is a 40% glass filled, pigmented black, injection molding PA6 grade. |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature 23.0 °C |
50.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Akro-Plastic Akromid® B3 GF 30 (2472) PA 6 Conditioned, 30% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature 23.0 °C |
50.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
BASF Ultramid® B35EG3 15% Glass Filled PA6 (Conditioned) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature 23.0 °C |
50.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
BASF Ultramid® B35EG3 BK 00564 15% Glass Filled PA6 (Conditioned) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature 23.0 °C |
50.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
BASF Ultramid® B3EG3 15% Glass Filled PA6 (Conditioned) Description: 15% glass-fiber reinforced injection-molding grade with enhanced impact resistance, for example, for vehicle mirror housings as well as for the wheels of mountain bikes.Information prov.. |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature 23.0 °C |
50.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
BASF Ultramid® B3EG3 BK 00564 15% Glass Filled PA6 (Conditioned) Description: 15% glass-fiber reinforced injection-molding grade with enhanced impact resistance, for example, for vehicle mirror housings as well as for the wheels of mountain bikes.Information prov.. |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature 23.0 °C |
50.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
BASF Ultramid® B3EG5 25% Glass Filled PA6 (Conditioned) Description: 25% glass-fiber reinforced injection-molding grade for industrial articles and electrical insulating partsInformation provided by BASF |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature 23.0 °C |
50.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6600/58 GV 30 HWCP 30% Glass Fiber Nylon 66, Impact Modified Until -40°C, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact Unnotched | 10.5 J/cm² | 50.0 ft-lb/in² | ISO 179 |
BASF Ultramid® B3WG6 CR BK 23210 15% Glass Filled (Conditioned) Description: Ultramid B3WG6 CR BK23210 s a 30% glass fiber reinforced, heat stabilized injection molding PA6 grade for crash relevant applications.Information provided by BASF |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature -30.0 °C |
50.0 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eU |
DuPont Performance Polymers Zytel® EFE7374 BK416 Nylon 6
(Unverified Data**) 40% Glass Reinforced Toughened Polyamide 6 Zytel EFE7374 is a 40% fiber reinforced heat stabilized lubricated toughened polyamide 6 for injection molding. It has an improved impact resistance and ex.. |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature 23.0 °C |
50.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
BASF Ultramid® B3WG5 25% Glass Filled PA6 (Conditioned) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |