Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 9.00 J/cm² @Temperature 23.0 °C |
42.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
PolyOne Bergamid™ A70 G50 HW SO Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | ISO 179/1eU |
Pasargad Polymer Peyvand Pasamid 3P-H1150B Nylon 6, 50% Glass Fiber Reinforced Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Electrical PartsFastenerHousingInformation provided by Pasargad Polymer Peyvand Co |
|||
Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | flatwise; ISO 179 1fU |
Lehmann & Voss LUVOCOM® 50-8300 Polycarbonate, with PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High dimensionally stable precision parts, even at elevated te.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYL® A 218 V35 Black 21NHFE PA66, 35% glass fiber, Conditioned Description: TECHNYL® A 218 V35 BLACK 21NHFE is polyamide 6.6, high flow, reinforced with 35% glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefit.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² @Temperature -30.0 °C |
42.8 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Styrolution Luran® S 778 T ASA Luran S 778 T is an injection molding ASA grade with enhanced toughness and heat resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | ISO Data, Low Temp |
Styron Magnum™ 2610 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | ISO Data |
Styron Pulse® 959 ABS + Polycarbonate, 10% Glass Reinforced PULSE® 959 Engineering resin is a 10% glass reinforced resin designed to provide excellent processability, high heat resistance, and practical toughness. PULSE 959 Engineering resin has been used.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² @Temperature 23.0 °C |
42.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6000 GX 350 HWCP Combination Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® GV-4 FWA black 9225 PA*-GF40 Product description: Grivory GV-4 FWA black 9225 is a 40% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copol.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² @Temperature 30.0 °C |
42.8 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® GVL-5H black 9839 PA*-GF50 Product description: Grivory GVL-5H black 9839 is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long glass fibers. Grivory GVL-5H.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² @Temperature 30.0 °C |
42.8 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® HT3Z LF black 9564 PA* Product description: Grivory HT3Z LF is an unreinforced and impact resistant, PTFE modified engineering thermoplastic based on semi crystalline partially aromatic copolyamide. This Grivory HT produc.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² @Temperature 30.0 °C |
42.8 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® LV-30H FWA black 9225 PA12-GF30 Product description: Grilamid LV-30H FWA black 9225 is a 30 % glass fiber reinforced, heat stabilized polyamide12 injection molding grade with the following special features: Stiffness combined with.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² @Temperature 30.0 °C |
42.8 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® LV-30H FWA nat PA12-GF30 Product description: Grilamid LV-30H FWA natural is a 30 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: Stiffness combined with h.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® XE 4106 black 9992 PA612-GF30 Product description: Grilamid XE 4106 black 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4106 are: low water absorpti.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² @Temperature 30.0 °C |
42.8 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® XE 5107 (GVL-5H V0) PA*-GF50 Product description: Grivory XE 5107 black 9915 is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide. The product is flame retarded and reinf.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² @Temperature -30.0 °C |
42.8 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eU |
DuPont Performance Polymers Zytel® 73G35HSL BK262 Nylon 6
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G35HSL BK262 is a 35% glass fiber reinforced heat stabilized black polyamide 6 resin for injection molding.Information provided by DuPont Per.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² @Temperature -30.0 °C |
42.8 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® FG70G50HSLA BK309 Nylon 66
(Unverified Data**) 50% Glass Reinforced Heat Stabilized Polyamide 66 with Developed for Food Contact Applications Information provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | 50%RH; ISO 179/1eU |
DuPont Performance Polymers Zytel® FG77G33L NC010 Nylon 612 33% Glass Reinforced Polyamide 612 with Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 9.00 J/cm² @Temperature 30.0 °C |
42.8 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® BG-50 H PA6-GF50 Product description: Grilon BG-50 H is a high heat stabilized PA6 injection molding grade with 50% glass fibers. Grilon BG-50 H has the following important properties: High stiffnessHigh heat resist.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² @Temperature 30.0 °C |
42.8 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® GVL-6H black 9839 PA*-GF60 Product description: Grivory GVL-6H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long glass fibers. Grivory GVL-6H blac.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | dry; ISO 179 1eU |
Azoty Tarnow™ Tarnamid® T-27 GF30 TF15 Polyamide 6 - Improved Slip Properties Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Low wear and low friction grade, contains molybdenum disulfide, PTFE.Tarnamid.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² @Temperature 23.0 °C |
42.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Akro-Plastic Akroloy® PA GF 40 (2845) PA 6.6 & PA6I/6T Conditioned, 40% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² @Temperature 23.0 °C |
42.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Akro-Plastic Akromid® A3 GF 25 (2420) PA 6.6 Conditioned, 25% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² @Temperature 23.0 °C |
42.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Akro-Plastic Akromid® B3 GF 25 (2471) PA 6 Conditioned, 25% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | ISO 179 |
BASF Ultramid® 8234G HS 44% Glass Filled PA6 (Dry) Ultramid 8234G HS is a heat stabilized, 44% glass fiber reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensio.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² @Temperature 30.0 °C |
42.8 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® XE 4192 black 9992 PA610-GF30 Information provided by EMS Grivory |