Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | ISO 179/1eU |
Pasargad Polymer Peyvand Pasamid 3P-H1135B Nylon 6, 35% Glass Fiber Reinforced Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Electrical PartsFastenerHousingInformation provided by Pasargad Polymer Peyvand Co |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 50-7317 Polycarbonate, with PTFE, easy flowing Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | |
LATI Laramid G/45 PPA, 45% Glass Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; .. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 23.0 °C |
40.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eU |
Gromax BFG30-BN00N1 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYL® A 60 G1 V25 PA66, 25% glass fiber, Conditioned Description: TECHNYL® A 60G1 V25 is a 25% GF reinforced organophosphorous flame retarded grade based on a patented high flow polyamide 66 resin. This product is heat stabilized and provides optim.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYL® C 216 V45 PA6, 45% glass fiber, Conditioned Description: Polyamide PA6, reinforced with 45% of glass fiber, for injection molding.Available in: EuropeProduct Applications: TECHNYL C 216 V45 has been optimized to have high impact strength, a n.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYLSTARâ„¢ SX 216 V60 PA6, 60% glass filled, DRY Description: TECHNYL STAR TM Polyamide reinforced with 60% of glass fiber, for injection molding. Characterized by a high fluidity of the melt.Available in: Europe and North America Product Applicat.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYLSTARâ„¢ SX 218 V50 PA6, 50% glass filled, DRY Description: TECHNYLSTARâ„¢ SX 218 V50 is based on a patented high flow polyamide 6 resin (Technylstar), heat stabilized, reinforced with 50% of glass fiber, for injection molding. This product i.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 23.0 °C |
40.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Borealis MB250WG Polypropylene Compound, Mineral Filled MB250WG is a 20 % mineral filled polypropylene compound intended for injection molding. Applications: MB250WG has been developed especially for the white goods industry. Washing machine parts, and .. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | ISO 179-1 |
Unitika A1030GFL PA6, 30% Glass Fiber Reinforced, Conditioned Information provided by Unitika Ltd. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 30.0 °C |
40.4 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® 1SVX-50H black 9288 PA1010-GF50 Product Description: Grilamid 1SVX-50H black 9288 is a 50% glass fiber reinforced Polyamide 1010 injection molding grade with the following product profile. Key properties of Grilamid 1SBVX-50H LDS .. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 30.0 °C |
40.4 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® 1SVX-50H nat PA1010-GF50 Product Description: Grilamid 1SVX-50H natural is a 50% glass fiber reinforced Polyamide 1010 injection molding grade with the following product profile: Raw materials based on renewable resources E.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® BG-15/2 PA6-GF15 Product description: Grilon BG-15/2 is a heat stabilized PA6 injection molding grade with 15% glass fibers. Grilon BG-15/2 has the following important properties: Good surface finishEasy processingG.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® BG-30 PA6-GF30 Product description: Grilon BG-30 is a heat stabilized PA6 injection molding grade with 30% glass fibers. Grilon BG-30 has the following important properties: High stiffnessGood balance between stre.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® LVX-65H SST black 9288 PA12-GF65 Product description: Grilamid LVX-65H SST black 9288 is a 65% glass fiber reinforced, heat stabilized engineering thermoplastic based on polyamide 12 for complex structural parts with the following .. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® TSG-35/4 PA666-GF35 Product description: Grilon TSG-35/4 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 35% glass fibers. Grilon TSG-35/4 has the following important properties: Good flo.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® TSG-35/4 W black 9832 PA666-GF35 Product description: Grilon TSG-35/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 35% glass fibers, modified for parts with high thermal demands. Grilon TSG-.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® TSG-50/4 FA PA666-GF50 Information provided by EMS Grivory |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® TSK-30/4 PA666-GB30 Product description: Grilon TSK-30/4 is a heat stabilized, normal viscosity PA66 +PA6 injection molding grade with 30% glass beads. Grilon TSK-30/4 has the following important properties: Good surfa.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® XE 3915 PA12-GF50 Product description: Grilamid XE 3915 is a 50% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following produce profile:Good UV StabilityHigh impact strengthVe.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 30.0 °C |
40.4 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® XE 3915 PA12-GF50 Product description: Grilamid XE 3915 is a 50% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following produce profile:Good UV StabilityHigh impact strengthVe.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 30.0 °C |
40.4 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® XE 4104 black 9992 PA610-GF40 Product description: Grilamid XE 4104 black 9992 is a 40% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw mate.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 30.0 °C |
40.4 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® XE 4104 nat PA610-GF40 Product description: Grilamid XE 4104 natural is a 40% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw materia.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® XE 4107 black 9992 PA612-GF40 Product description: Grilamid XE 4107 black 9992 is a 40% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4107 are: low water absorpti.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 30.0 °C |
40.4 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® XE 4107 black 9992 PA612-GF40 Product description: Grilamid XE 4107 black 9992 is a 40% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4107 are: low water absorpti.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | Edgew 80x10x4 sp=62; ISO 179/1eU |
Eurostar Staramide PF00AS PA6, 50% Glass Fiber Filled, Injection Molded Staramide PF00AS is a 50% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 30.0 °C |
40.4 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® BGZ-30 PA6-GF30 Product description: Grilon BGZ-30 is a normal viscosity, heat stabilized and impact modified PA 6 injection molding type with 30% glass fibers. Grilon BGZ-30 has the following important properties:.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 30.0 °C |
40.4 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® GVL-6H black 9915 PA*-GF60 Product description: Grivory GVL-6H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long glass fibers. Grivory GVL-6H blac.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 30.0 °C |
40.4 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® GVN-5H black 9915 PA*-GF50 Product description: Grivory GVN-5H is a 50 % glass-fiber reinforced, impact-modified engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic c.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | cond.; ISO 179 1eU |
Azoty Tarnow™ Tarnamid® T-27 GF15 I Polyamide 6 - Glass Fiber Reinforced 15% Glass fiber reinforced, impact modified, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following mai.. |