Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 8.20 J/cm² | 39.0 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Lexan® 144 PC UL rated HB. 200 series recommended when V-2 rating required. 10.5 MFR. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will no longer be supported with bioco.. |
|||
Charpy Impact Unnotched | 8.20 J/cm² | 39.0 ft-lb/in² | ISO 179/1eU |
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0.. |
|||
Charpy Impact Unnotched | 8.20 J/cm² | 39.0 ft-lb/in² | Type 1, Edgewise; ISO 179 |
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater th.. |
|||
Charpy Impact Unnotched | 8.20 J/cm² @Temperature 23.0 °C |
39.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179; DIN 53453 |
Zell-Metall Engineering Plastics Zellamid 1400 (PET) Zellamid® 1400 is the registered trademark of Zell-Metalls partly crystalline thermoplastic Polyester based on Polyethylene Terephthalate.This PETP features outstanding dimensional stability, .. |
|||
Charpy Impact Unnotched | 8.20 J/cm² @Temperature 23.0 °C |
39.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179; DIN 53453 |
Zell-Metall Engineering Plastics Zellamid 1400 (PET) at 50% RH Zellamid® 1400 is the registered trademark of Zell-Metalls partly crystalline thermoplastic Polyester based on Polyethylene Terephthalate.This PETP features outstanding dimensional stability, .. |
|||
Charpy Impact Unnotched | 8.20 J/cm² | 39.0 ft-lb/in² | ISO 179-1 |
Unitika A1030TF PA6, Dry Lubricating nylonInformation provided by Unitika Ltd. |
|||
Charpy Impact Unnotched | 8.20 J/cm² @Temperature -30.0 °C |
39.0 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Covestro Desmopan® DP 3970D Polyurethane, 20% Glass Filled injection molding grade20 % Glass fiber reinforcedgood heat resistancelow coefficent of linear thermal expansionApplicationAutomotive engineeringInjection molded engineering partsPreprocessingMax. W.. |
|||
Charpy Impact Unnotched | 8.20 J/cm² | 39.0 ft-lb/in² | DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® 70G30HSL NC010 Nylon 66
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G30HSL NC010 is a 30% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perform.. |
|||
Charpy Impact Unnotched | 8.20 J/cm² @Temperature 23.0 °C |
39.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6000 GV 25 HWCP 25% Glass Fiber Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact Unnotched | 8.20 J/cm² @Temperature 23.0 °C |
39.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6000 GV 25 HWUVCP 25% Glass Fiber Nylon 6, UV Stabilized, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact Unnotched | 8.20 J/cm² @Temperature 23.0 °C |
39.0 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® HTN 54G35EF NC010 Polyphthalamide (PPA) Zytel® HTN54G35EF NC010 is a 35% glass reinforced, toughened, heat stabilized, lubricated high performance polyamide resin, developed for electrical and electronics applications. It is also a PPA r.. |