Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO Data, Low Temp |
Americas Styrenics Styron® 489M High Impact Polystyrene
(discontinued **) STYRON® 489M high impact polystyrene resin is a high flow resin with excellent impact. When used unmodified for the manufacture of food contact articles STYRON 489M complies with the US Food, Drug .. |
|||
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 20-0791 Polyphthalamide, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² @Temperature -30.0 °C |
38.1 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Lehmann & Voss LUVOCOM® 50/TF/15/BK Polycarbonate, with PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYL® B 216 V30 Black 3 N PA66, 30% glass fiber, DRY Description: Copolyamide 66/6, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific and EuropeProduct Applications: TECHNYL® B 216 V30 is used in all sectors of in.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | Type 1, Edgewise; ISO 179 |
Solvay Specialty Polymers Amodel® AE-8950 Polyphthalamide (PPA), 50% Glass Fiber Amodel® AE-8950 is a 50% glass reinforced polyphthalamide (PPA) designed to work in the modern automotive electrical environment. Features: Glycol Resistant; Good Chemical Resistance; Good Creep .. |
|||
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO 179 |
Solvay Specialty Polymers Amodel® DW-1150 Polyphthalamide (PPA), 50% Glass Fiber Amodel® DW-1150 is a 50% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient o.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² @Temperature -30.0 °C |
38.1 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Styrolution Terlux® 2802 TR MABS Terlux 2802 TR is a standard injection molding MABS grade for tranparent parts.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO Data, Low Temp |
Styron Magnum™ 2645 ABS, Impact Grade MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® BGZ-30/2 PA6-GF30 Product description: Grilon BGZ-30/2 is a heat stabilized and impact modified PA6 injection molding grade with 30% glass fibers. Grilon BGZ-30/2 has the following important properties: Good impact s.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® EBV-2H PA6-GF20 Product description: Grilon EBV-2H is a high viscosity, heat stabilized PA6 extrusion blow molding grade with 20% glass fibers. Grilon EBV-2H has the following important properties: High melt streng.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² @Temperature 30.0 °C |
38.1 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® GV-5H EF black 9915 PA*-GF50 Product description: Grivory GV-5H black 9915 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² @Temperature 30.0 °C |
38.1 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® GV-6 FWA nat PA*-GF60 Product description: Grivory GV-6 FWA natural is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² @Temperature 30.0 °C |
38.1 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® GVN-35H black 9915 PA*-GF35 Product description: Grivory GVN-35H is a 35% glass-fiber reinforced, impact-modified engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic c.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² @Temperature 30.0 °C |
38.1 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® HT3Z black 9564 PA* Product description: Grivory HT3Z is an unreinforced and impact resistant, engineering thermoplastic based on semi crystalline partially aromatic copolyamide. This Grivory HT product is partially ba.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® LV-30H FWA nat PA12-GF30 Product description: Grilamid LV-30H FWA natural is a 30 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: Stiffness combined with h.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² @Temperature 30.0 °C |
38.1 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® LV-50H FWA nat PA12-GF50 Product description: Grilamid LV-50H FWA natural is a 50 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combined w.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® TSG-30/4 FA PA666-GF30 Information provided by EMS Grivory |
|||
Charpy Impact Unnotched | 8.00 J/cm² @Temperature 30.0 °C |
38.1 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® TSG-50 FA PA666-GF50 Information provided by EMS Grivory |
|||
Charpy Impact Unnotched | 8.00 J/cm² @Temperature 30.0 °C |
38.1 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® TSG-50/4 FA PA666-GF50 Information provided by EMS Grivory |
|||
Charpy Impact Unnotched | 8.00 J/cm² @Temperature 30.0 °C |
38.1 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® TSGL-50/4 black 9833 PA666-GF50 Product description: Grilon TSGL-50/4 black is based on a heat stabilized semicrystalline Polyamide PA66+PA6 and 50% long glass fibers. Grilon TSGL-50/4 black is characterized by the following key-p.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® HT1V-5 HY black 9205 PA6T/6I-GF50 Product description: Grivory HT1V-5 HY black 9205 is a 50% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT1V-5 HY bl.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² @Temperature -30.0 °C |
38.1 ft-lb/in² @Temperature -22.0 °F |
|
BASF Polystyrol® 585 K Impact Grade Polystyrene (Europe) Special high gloss, high-impact grade for all types of housings. Basis product for gloss capping.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 8.00 J/cm² - NB | 38.1 ft-lb/in² - NB | Average value: 9.40 J/cm² Grade Count:6 |
Overview of materials for Nylon 6, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, PTFE Filled". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² @Temperature 23.0 °C |
38.1 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® 74G33W BK196 Nylon 66
(Unverified Data**) Zytel® 74G33W BK196 is a high gloss automotive weatherable black 33% glass reinforced nylon 66 and nylon 6 comelt resin.Information provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | 50%RH; ISO 179/1eU |
DuPont Performance Polymers Zytel® 70G30HSL BK039B Nylon 66
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Polyamide 66 Information provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 8.00 J/cm² @Temperature 30.0 °C |
38.1 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® GV-5 FWA nat PA*-GF50 Product description: Grivory GV-5 FWA natural is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² @Temperature 30.0 °C |
38.1 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® GV-5 FWA nat PA*-GF50 Product description: Grivory GV-5 FWA natural is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² @Temperature 30.0 °C |
38.1 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® GV-6H EF nat PA*-GF60 Product description: Grivory GV-6H EF black 9915 is a 60% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copol.. |