Mechanical Properties Metric English Comments
Charpy Impact Unnotched 6.40 J/cm²

@Temperature 23.0 °C
30.5 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
DuPont Performance Polymers Rynite® 408 BK515 PET
Rynite® 408 BK515 is a 30% glass reinforced modified polyethylene terephthalate with improved impact resistance. Excellent balance of strength, stiffness, toughness and temperature resistance.Info..
Charpy Impact Unnotched 6.40 J/cm²
30.5 ft-lb/in²
Arkema Group Rilsan® AZM 15 TLD Nylon 12, 15% Glass Fiber Filled (Conditioned)
Designation ISO 1874-PA12,MHLR,16-030,GF15Rigid grade with glass fiber filler (15%) for injection molding.Available color: natural. Light and heat stabilized. Mold-release agent.Rigidity combined wi..
Charpy Impact Unnotched 6.40 J/cm²

@Temperature -30.0 °C
30.5 ft-lb/in²

@Temperature -22.0 °F
ISO 179
BASF Ultradur B 4040 G10 LS High Speed BK15029 50% Glass Filled PBT/PET