Mechanical Properties Metric English Comments
Charpy Impact Unnotched 2.75 J/cm²
13.1 ft-lb/in²
ISO 179/1eU
NOVA Chemicals DYLARK® 480P16 Glass Reinforced Engineering Resin
Features:Very high modulus High heat resistance Excellent flow characteristics Excellent adhesion to urethaneApplications:Instrument panel substrates Consoles Cluster housings Interior trimInformati..
Charpy Impact Unnotched 2.75 J/cm²
13.1 ft-lb/in²
ISO 179
GEHR Plastics PEEK-mod Polyetheretherketone, 10% PTFE, 10% Graphite, 10% Carbon Fiber
Polyether etherketone can be used at very high temperatures and it shows a good mechanical strength, toughness, hardness, flexural strength, and torsional strength. PEEK exhibits excellent chemical ..