Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 0.400 - 0.600 J/cm² @Temperature 23.0 °C |
1.90 - 2.86 ft-lb/in² @Temperature 73.4 °F |
Injection and Compression; ISO 179/ 1eU |
Raschig Group 4552 Silicone Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to +/- 300°C continuously, excellent electrical properties, good mechanical strength, very good dimensional stabi.. |
|||
Charpy Impact Unnotched | 0.400 - 0.600 J/cm² | 1.90 - 2.86 ft-lb/in² | Injection; ISO 179/1eU |
Raschig Group 4554 Silicone Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to 300°C, exceptional electrical properties, good mechanical strength, very good dimensional stability. Processi.. |
|||
Charpy Impact Unnotched | 0.400 - 0.600 J/cm² | 1.90 - 2.86 ft-lb/in² | Compression; ISO 179/1eU |
Raschig Group 6551 DAIP Diallyl Phthalate (DAP), Cast, Mineral Filler Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi.. |
|||
Charpy Impact Unnotched | 0.400 - 0.600 J/cm² | 1.90 - 2.86 ft-lb/in² | Compression; ISO 179/1eU |
Raschig Group DECAL® 5431 Phenolic Organically and inorganically filled phenolic molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/.. |
|||
Charpy Impact Unnotched | 0.400 - 0.600 J/cm² @Temperature 23.0 °C |
1.90 - 2.86 ft-lb/in² @Temperature 73.4 °F |
Injection and Compression; ISO 179/ 1eU |
Raschig Group EPOXIDUR® 3580 EP Epoxy Glass-fiber reinforced and mineral filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties even with thin wall thicknesses and high temperatures. This prod.. |
|||
Charpy Impact Unnotched | 0.400 - 0.700 J/cm² | 1.90 - 3.33 ft-lb/in² | Compression; ISO 179/1eU |
Raschig Group MELOPAS® 156 MF Melamine Glass fiber reinforced Melamine molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 200.. |
|||
Charpy Impact Unnotched | 0.400 - 0.600 J/cm² | 1.90 - 2.86 ft-lb/in² | Compression; ISO 179/1eU |
Raschig Group RALUPOL® 5000 UP Polyester Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, excellent heat resistance, good mechanical strength. This product meets the all.. |
|||
Charpy Impact Unnotched | 0.400 - 5.00 J/cm² @Temperature -40.0 - -20.0 °C |
1.90 - 23.8 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 2.36 J/cm² Grade Count:4 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Charpy Impact Unnotched | 0.400 - 2.50 J/cm² | 1.90 - 11.9 ft-lb/in² | Average value: 1.38 J/cm² Grade Count:4 |
Overview of materials for Silicone, Molded, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val.. |
|||
Charpy Impact Unnotched | 0.400 - 1.50 J/cm² | 1.90 - 7.14 ft-lb/in² | Average value: 0.928 J/cm² Grade Count:10 |
Overview of materials for Phenolic, Novolac, Mineral/Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Glass Filled". Each property range of values reported is minimum and maximum .. |
|||
Charpy Impact Unnotched | 0.400 J/cm² @Temperature 23.0 °C |
1.90 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eU |
Gromax BPR20-N1 Nylon 6, Flame Retardant (Dry) Information provided by Gromax Enterprises Corp. |
|||
Charpy Impact Unnotched | 0.400 J/cm² | 1.90 ft-lb/in² | |
LATI Laticonther 52/11 CP3/600 F3 PP Homopolymer High thermal conductivity product based on Polypropylene homopolymer (PPh). Special filler. Potentially suitable for food/medical contact application.Availability: Africa & Middle East; Asia Pacific.. |
|||
Charpy Impact Unnotched | 0.400 J/cm² | 1.90 ft-lb/in² | |
LATI Laticonther 52/11 GR/70 PP Homopolymer High thermal conductivity product based on Polypropylene homopolymer (PPh). Graphite.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lat.. |
|||
Charpy Impact Unnotched | 0.400 J/cm² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
|
Styrolution NOVODUR® P2HGV ABS, 16% Glass Fiber Injection molding grade, glass reinforced (16%).Applications: Automotive industry: instrument panels, rear light housings, internal components of domestic appliances. |
|||
Charpy Impact Unnotched | 0.400 - 0.600 J/cm² | 1.90 - 2.86 ft-lb/in² | ISO 179 |
Vyncolit X658 Novolac Phenolic Glass fiber and mineral filled phenolic molding compound with excellent mechanical and thermal properties and a very good dimensional stability.USES: Complex precision parts.Information provided by .. |
|||
Charpy Impact Unnotched | 0.400 J/cm² | 1.90 ft-lb/in² | IS0179-1:2000 |
Zhejiang Juner PP201-G30 PP For Automotive Parts Applications: FansInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Charpy Impact Unnotched | 0.400 J/cm² @Temperature -20.0 °C |
1.90 ft-lb/in² @Temperature -4.00 °F |
Notched/Unnotched not specified; ASTM DIN53453 |
Total PPC 4720 WZ Polypropylene, Impact Copolymer ATOFINA 4720 is an impact copolymer. 4720 is characterized by a high fluidity offering a combination of east of processing and good mechanical properties.ApplicationATOFINA 4720 has been formulated.. |
|||
Charpy Impact Unnotched | 0.400 J/cm² - NB | 1.90 ft-lb/in² - NB | Average value: 7.75 J/cm² Grade Count:49 |
Overview of materials for Nylon 6, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v.. |
|||
Charpy Impact Unnotched | 0.400 J/cm² @Temperature 23.0 °C |
1.90 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
LATI LARTON CE/60 60% Special Mineral Filled Polyphenylene sulfide (PPS)
(Unverified Data**) Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex.. |
|||
Charpy Impact Unnotched | 0.400 J/cm² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
|
Ineos ABS NOVODUR® P3T ABS, Injection Grade
(discontinued **) Injection molding grade, higher heat resistance.Applications: Automotive industry.Information provided by the manufacturer.Novodur is produced by Styrolution (2014). This grade was discontinued pri.. |
|||
Charpy Impact Unnotched | 0.400 - 6.00 J/cm² | 1.90 - 28.6 ft-lb/in² | Average value: 2.56 J/cm² Grade Count:22 |
Overview of materials for Epoxy, Molded, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values.. |
|||
Charpy Impact Unnotched | 0.400 - 0.700 J/cm² @Temperature -40.0 - -40.0 °C |
1.90 - 3.33 ft-lb/in² @Temperature -40.0 - -40.0 °F |
Average value: 0.550 J/cm² Grade Count:1 |
Overview of materials for Melamine-Phenolic Copolymer This property data is a summary of similar materials in the MatWeb database for the category "Melamine-Phenolic Copolymer". Each property range of values reported is minimum and maximum values of ap.. |
|||
Charpy Impact Unnotched | 0.400 - 1000 J/cm² | 1.90 - 4760 ft-lb/in² | Average value: 0.975 J/cm² Grade Count:5 |
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Unreinforced, Extruded". Each property range of values reported is minimum .. |
|||
Charpy Impact Unnotched | 0.400 - 8.70 J/cm² @Temperature -40.0 - -20.0 °C |
1.90 - 41.4 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 4.42 J/cm² Grade Count:56 |
Overview of materials for Polypropylene with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i.. |