Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 1.40 - 9.00 J/cm² @Temperature -30.0 - -30.0 °C |
6.66 - 42.8 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 6.55 J/cm² Grade Count:8 |
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi.. |
|||
Charpy Impact Unnotched | 1.50 - 9.00 J/cm² | 7.14 - 42.8 ft-lb/in² | Average value: 4.07 J/cm² Grade Count:9 |
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi.. |
|||
Charpy Impact Unnotched | 4.00 - 9.00 J/cm² @Temperature -30.0 - -30.0 °C |
19.0 - 42.8 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 6.47 J/cm² Grade Count:10 |
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m.. |
|||
Charpy Impact Unnotched | 2.00 - 9.00 J/cm² @Temperature -30.0 - 30.0 °C |
9.52 - 42.8 ft-lb/in² @Temperature -22.0 - 86.0 °F |
Average value: 4.20 J/cm² Grade Count:26 |
Overview of materials for Nylon 6, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Charpy Impact Unnotched | 2.50 - 9.00 J/cm² | 11.9 - 42.8 ft-lb/in² | Average value: 5.50 J/cm² Grade Count:3 |
Overview of materials for Nylon 6, Glass Fiber/Solid Lube Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber/Solid Lube Filled". Each property range of values reported is minimum and maximum v.. |
|||
Charpy Impact Unnotched | 4.00 - 9.00 J/cm² @Temperature -30.0 - -20.0 °C |
19.0 - 42.8 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 7.25 J/cm² Grade Count:6 |
Overview of materials for Nylon 66/Nylon 6 Blend, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/Nylon 6 Blend, Glass Fiber Filled". Each property range of values reported is minimum and maxim.. |
|||
Charpy Impact Unnotched | 2.40 - 9.00 J/cm² @Temperature -40.0 - -20.0 °C |
11.4 - 42.8 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 4.51 J/cm² Grade Count:28 |
Overview of materials for Nylon 66, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |
|||
Charpy Impact Unnotched | 2.20 - 9.00 J/cm² @Temperature -40.0 - -30.0 °C |
10.5 - 42.8 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 4.59 J/cm² Grade Count:16 |
Overview of materials for Nylon 66, 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc.. |
|||
Charpy Impact Unnotched | 2.30 - 9.00 J/cm² | 10.9 - 42.8 ft-lb/in² | Average value: 5.30 J/cm² Grade Count:10 |
Overview of materials for Nylon 66, 30% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in.. |
|||
Charpy Impact Unnotched | 2.00 - 9.00 J/cm² | 9.52 - 42.8 ft-lb/in² | Average value: 4.88 J/cm² Grade Count:24 |
Overview of materials for Nylon 66, Glass/Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Charpy Impact Unnotched | 3.80 - 9.00 J/cm² | 18.1 - 42.8 ft-lb/in² | Average value: 6.26 J/cm² Grade Count:30 |
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40% This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. .. |
|||
Charpy Impact Unnotched | 3.20 - 9.00 J/cm² @Temperature -20.0 - 0.000 °C |
15.2 - 42.8 ft-lb/in² @Temperature -4.00 - 32.0 °F |
Average value: 6.10 J/cm² Grade Count:2 |
Overview of materials for Polypropylene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of.. |
|||
Charpy Impact Unnotched | 4.50 - 9.00 J/cm² @Temperature -30.0 - -20.0 °C |
21.4 - 42.8 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 6.50 J/cm² Grade Count:7 |
Overview of materials for Polypropylene with 60% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 60% Glass Fiber Filler". Specific grades with glass content between 55% and 64% are i.. |