Charpy Impact Unnotched 3.50 - 6.40 J/cm²
16.7 - 30.5 ft-lb/in²
Average value: 4.79 J/cm² Grade Count:23
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum ..
Charpy Impact Unnotched 0.900 - 6.40 J/cm²

@Temperature -40.0 - -20.0 °C
4.28 - 30.5 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 1.77 J/cm² Grade Count:22
Overview of materials for Polypropylene with 40% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are..