Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 2.00 - 19.0 J/cm² @Temperature -30.0 - 30.0 °C |
9.52 - 90.4 ft-lb/in² @Temperature -22.0 - 86.0 °F |
Average value: 4.92 J/cm² Grade Count:32 |
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% .. |