Polymer Property : Charpy Impact Unnotched = 11.0 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 7.50 - 11.0 J/cm²
35.7 - 52.4 ft-lb/in²
Average value: 9.17 J/cm² Grade Count:39
Overview of materials for Nylon 610, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap..
Charpy Impact Unnotched 6.00 - 11.0 J/cm²

@Temperature -30.0 - 30.0 °C
28.6 - 52.4 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 8.87 J/cm² Grade Count:24
Overview of materials for Nylon 610, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap..
Charpy Impact Unnotched 2.00 - 11.0 J/cm²

@Temperature -30.0 - 30.0 °C
9.52 - 52.4 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 7.73 J/cm² Grade Count:19
Overview of materials for Nylon 612, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of ..
Charpy Impact Unnotched 2.50 - 11.0 J/cm²
11.9 - 52.4 ft-lb/in²
Average value: 8.05 J/cm² Grade Count:47
Overview of materials for Nylon 46, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values ..
Charpy Impact Unnotched 1.00 - 11.0 J/cm²

@Temperature -30.0 - -30.0 °C
4.76 - 52.4 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 6.00 J/cm² Grade Count:2
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum..